Dr. Brian Ikeda

Associate Professor
Faculty of Energy Systems and Nuclear Science
UOIT
2000 Simcoe Street North
Oshawa, ON L1H 7K4
Office: UA 3031
e-mail:
Brian.Ikeda@uoit.ca
Tel: 905.721.8668 ext. 2749
Fax: 905.721.3046
Education
-
PhD (Physical Chemistry), The University of
Newcastle upon Tyne,
UK
-
MSc (Chemistry),
University of
Guelph
-
BSc (Hons),
University of
Manitoba
Courses Taught
-
Corrosion for Engineers
-
Radioactive Waste Management - Design
Research Areas:
-
Corrosion of materials in molten fluoride salts
-
Electrochemical and physical degradation of fluorine anodes
-
Corrosion of nuclear waste container materials
-
Stress assisted corrosion cracking of metals
-
Localized corrosion of metals at elevated temperatures
-
Long-term performance assessment of materials
-
Radioactive waste management
Selected Publications:
Book Chapter
D.W. Shoesmith,
B.M. Ikeda and F. King, "Modelling Procedures for Predicting the Lifetimes of Nuclear Waste Containers", in Modelling Aqueous Corrosion, K.R. Trethewey andP.R. Roberge (Eds), NATO ASI Series, Kluwer, Boston, pp. 201-239, 1994
Journal Publications
F. King,
B.M. Ikeda and D.W. Shoesmith,"Nuclear Waste: Can We Contain It?" Chemtech.
22(4), 1992.
C.F. Clarke, D. Hardie and
B.M. Ikeda,"Hydrogen-Induced Cracking of Commercial Purity Titanium", Corrosion Science,
39(9),1545-1599, 1997.
D.A. Shoesmith, J.J. Noel, D. Hardie and
B.M.Ikeda. 2000. "Hydrogen Absorption and the Lifetime Performance of Titanium Nuclear Waste Containers. Corrosion Reviews,
18(4-5), 331‑359, 2000.
Technical Reports
B.M. Ikeda
,J.J. Noël, and D.W. Shoesmith, "Crevice Corrosion and the Lifetime Performance of Titanium Nuclear Fuel Waste Container", AECL-11823, COG-97-061-I,1997.
McMurry, J
.,
B.M. Ikeda, M.J.Quinn, S. Stroes-Gascoyne, C.J. Hamon and P. Vilks. 2001. Metallic Copper and Iron Artifacts in a Corrosive Depositional Environment: the Colony of Avalon Archaeological Analgoue in Ferry land,
Newfoundland.
Ontario Power Generation Report 06819-REP-01200-10070-R00.
B.M. Ikeda
and C.D. Litke. 2001. The Measurement of Corrosion Parameters on Oxygen-Free Phosphorous-Doped Copper in Nitrite Solution.
Ontario Power Generation Report, 06819-REP-01300-10033-R00.
J. McMurry,
B.M. Ikeda, S.Stroes-Gascoyne, and D.A. Dixon. 2004. Evolution of a Canadian Deep Geological Repository: Defective Container Scenario.
Ontario Power Generation Waste Management Division Report 06819‑REP‑01200‑10127‑R00.
Conference Presentations
J.J. Noël, D.W. Shoesmith and
B.M. Ikeda. "Crevice Corrosion of Alpha Titanium Alloys",in Proceedings of the Research Topical Symposia, NACE Corrosion/2001, Houston,TX, March 11‑16, 2001, G.S. Frankel, (ed)., NACE International, Houston, TX, (2001), pp. 65‑102.
B.M. Ikeda
, C.D.Litke and F. King, "Stress Corrosion Cracking of Pure Coppers in Nitrite/Chloride Mixtures" Extended Abstract presented at NACE International, 2001 Corrosion,
Houston,
TX, 2001 March.
B.M. Ikeda
andC.D. Litke. 2004. "Stress Corrosion Cracking of Pure Copper in Ammonia-Chloride Solutions". 87thCanadian Chemistry Conference, 2004 May,
London
ON.
Honours, Awards & Affiliations
-
Member of the Electrochemical Society
-
Member of the NACE
-
Member of the ASM
-
Cameco Research Chair in Nuclear Fuels